Compositon
|
|
Technical Specifications
|
|
Compositon
|
|
Technical Specifications
|
|
||||
Nickel
|
62%
|
Melting Range()
|
1335±50
|
Nickel
|
70%
|
Melting Range()
|
1335±50
|
||||
Chrome
|
23%
|
Yield Strength(MPa)
|
400
|
Chrome
|
18%
|
Yield Strength(MPa)
|
880
|
||||
Molybdenum
|
10%
|
Elongation(%)
|
14
|
Molybdenum
|
8%
|
Elongation(%)
|
3
|
||||
Silicon
|
2%
|
RockwellHardness
|
80
|
Beryllium
|
1.7%
|
Rockwell Hardness
|
80
|
||||
Others
|
3%
|
Coefficient Of Liner Expansion(25-500)
|
14
|
Others
|
2%
|
Coefficient Of Liner Expansion(25-500)
|
14
|
Compositon
|
|
Technical Specifications
|
|
Compositon
|
|
Technical Specifications
|
|
||||
Cobalt
|
60%
|
Melting Range()
|
1360±50
|
Cobalt
|
50%
|
Melting Range()
|
1350±50
|
||||
Chrome
|
26%
|
Yield Strength(MPa)
|
530
|
Chrome
|
25%
|
Yield Strength(MPa)
|
620
|
||||
Wolfram
|
10%
|
Tensile Strength(MPa)
|
880
|
Ferrum
|
15%
|
Tensile Strength(MPa)
|
810
|
||||
Molybdenum
|
4%
|
Elongation(%)
|
3
|
Molybdenum
|
5%
|
Elongation(%)
|
3
|
||||
Others
|
2%
|
Rockwell Hardness
|
30
|
Nickel
|
4%
|
Rockwell Hardness
|
30
|
||||
|
|
Coefficient Of Liner Expansion(25-500)
|
14.7
|
Others
|
2%
|
|
|